ASNT UT Level II UT Beam Techniques: What the Exam Tests

By Sandeep Bandyopadhyay, Engineer and founder of CertCrafter · PMP, MBA

TL;DR

ASNT publishes no weighting for beam techniques, but its topic list for UT exams after February 5, 2027 names zero-degree, angle beam, pulse echo and through transmission examinations, and the older outline covers bonded structures. The UT General exam is 50 items in 2 hours. Expect stems that give a part and a problem, then ask which beam, which setup or which scan position fits and why.

Original questions, not exam dumps. Every CertCrafter question is written from the published body of knowledge and the referenced codes. None is copied from a live exam, and CertCrafter is independent: not affiliated with or endorsed by any awarding body.

An ultrasonic flaw detector with its probe leads on a work bench
Photo: GE USM 35X DAC LEMO type NDT tool by Plenumchamber (Wikimedia Commons), Public Domain, via Wikimedia Commons.

Most candidates can name a straight beam and an angle beam. They lose marks when the stem describes a part and a flaw and asks which beam, from where, and why that position.

Beam technique questions are choices, and each choice has a geometric reason behind it.

Video: ASNT UT II — The ASNT Level II ultrasonic exam in sixty seconds. ASNT UT II — The ASNT Level II ultrasonic exam in sixty seconds. Watch on YouTube · CertCrafter
Image: video thumbnail, source: CertCrafter on YouTube (@certcrafters).

What does ASNT list for beam techniques?

Less than a textbook chapter, and enough to plan around. The examination page gives the UT General exam as 50 items in 2 hours. It publishes no percentages for any heading, so a weighting from another site is an estimate. Our certification guide explains how the central route differs from employer certification.

The outline for exams before February 5, 2027 hides techniques in broad headings: Review of Ultrasonic Techniques, Evaluation of Weldments and Evaluation of Bonded Structures. After that date, the verbs get specific. A technician performs UT exams for inherent, manufacturing and in-service discontinuities, with the examples written as zero-degree, angle beam, pulse echo and through transmission.

Our question banks file this area as Straight Beam, Angle Beam and Specialised Methods. That is our label, not an ASNT heading. The 2027 outline guide walks the change group by group.

Four rows from ASNT's examination page: the UT General exam is 50 items in 2 hours, the Specific exam is 40 items in 2 hours, the outline changes on February 5, 2027, and the new outline names zero-degree, angle beam, pulse echo and through transmission
What the exam page fixes for this domain. Illustration: CertCrafter, from ASNT NDT Level II Examinations: Information and Scheduling.

When do you use a straight beam, and when an angle beam?

Match the beam to the way the flaw is oriented. A straight beam travels normal to the surface, so it likes flaws that lie parallel to it: laminations, and wall thickness work. An angle beam enters the steel as a shear wave at a chosen angle, so it likes flaws that stand up across the beam, such as cracks and lack of fusion in a weld.

The weld is the classic case. You cannot scan a butt weld from the top, because the cap is in the way. So the probe sits on the plate beside the weld and the sound arrives from the side, at an angle. The UT physics guide covers the refraction behind that angle.

On a job, the technique is already chosen for you. The procedure names the probe, the angle and the scan plan, and the Level II applies it. The exam asks whether you understand why those choices were made.

Why is a weld root scanned at half skip?

Because the root is where the far surface meets the face of the joint, and at half skip the beam hits that corner on its first leg. Two surfaces at right angles form a corner trap, and a corner trap throws energy straight back along the way it came. That is why lack of penetration and root cracks light up so strongly.

One of our free questions asks for the technical reason a procedure requires half skip on a single-sided root with an angle beam probe. The distractors are tempting. The shorter path means less attenuation, which is true but is a side benefit. The near field is a property of the probe, not of the leg. Mode conversion happens at the far surface, but avoiding it is not the point. The corner trap is the answer.

Worked example: where does the probe sit for the root?

A single-V butt weld is welded from one side. The procedure calls for a shear wave probe at a stated angle and half skip on the root.

  1. Half skip means the beam reaches the far surface once, at the root. So the sound has travelled the full plate thickness, and the depth at that point equals the thickness.
  2. Surface distance equals depth times the tangent of the probe angle.
  3. Multiply the plate thickness by that tangent. The result is the distance along the surface from the probe’s exit point to the spot directly above the root.
  4. Full skip puts the beam back at the top surface at twice that distance, so the root is not at full skip.
  5. Set the probe so its exit point sits that distance from the root line. Measure from the exit point, not from the front of the wedge.

The last step is the usual slip. A stem may give the distance from the front of the wedge and ask for the exit point. Read what is measured from where.

The Complete Exam Kit works more of these under timed conditions, with every answer explained.

An ultrasonic rail testing car, a vehicle built around probes
Photo: Korail Ultrasonic Rail Testing Car US2 KNR by Minseong Kim (Wikimedia Commons), CC BY-SA 4.0, via Wikimedia Commons.

How do you test a bonded panel?

With through transmission, not pulse echo. Picture an aluminium honeycomb panel with thin epoxy skins that has to be checked for disbonds.

In pulse echo, a thin facesheet rings. The multiples from it crowd the part of the timebase where the bond line signal would sit. Through transmission avoids the problem: one probe sends from one face, the other receives on the opposite face, and the measurement is how much energy gets across. A disbond or a crushed core blocks the path and shows as a drop in transmitted amplitude.

Another of our free questions tests this, and its wrong options are plausible. A shear wave probe on the skin sounds clever, but shear waves are attenuated in adhesives and do not couple into an air-filled core. A longer delay line moves the interface echo and leaves the facesheet ringing. Gating a third back wall echo assumes clean multiples through a panel that barely returns a first one.

A shear beam from a probe beside a weld in a plate, reaching the root corner at half skip and returning to the top surface at full skip
Why the root is scanned on the first leg. Illustration: CertCrafter, from ASNT NDT Level II Examinations: Information and Scheduling.

What do crews get wrong with beam technique in the field?

They scan the wrong leg. A flaw seen on the second leg is a different depth and a different surface distance from the same indication on the first leg, and a tired technician logs the wrong one. Marking the scan lines on the plate before the first pass costs a minute and saves a re-shoot.

They also trust a single angle on a weld with a flaw that does not face the beam. A crack tilted away from the beam can return almost nothing. This is why procedures name more than one angle, and why a limitation, such as a support saddle covering part of a seam, belongs in the report.

How do candidates lose marks in this domain?

First, by picking the true statement that is not the reason. Shorter paths do lose less energy, but the exam asks why half skip, and the answer is the corner.

Second, by measuring from the wrong point. Surface distance runs from the exit point.

Third, by reaching for pulse echo out of habit. When the facesheet rings, the technique has to change.

Fourth, by treating gain as a fix. Raising it lifts noise and signal together.

How should you study it?

Sketch each technique once with a part, a flaw orientation and the beam path. Then say aloud why that beam suits that flaw. Try the free ten-question sample and read every explanation, including the ones you got right. The equipment and calibration guide covers the probes that go with these techniques, and the study guides hub lists the rest. Our channel also has a short video: the ASNT Level II ultrasonic exam in sixty seconds.

Tonight, draw a one-sided butt weld, mark half skip and full skip, and check where the root falls.

Try these free questions

  1. A weld procedure requires the root of a single-V butt weld, welded from one side only, to be scanned at half skip with a 60 degree shear probe. What is the technical reason behind that instruction?

    1. Half skip gives the shortest sound path, so attenuation losses are at their lowest for the root region
    2. At half skip the beam meets the root corner square on, forming a strong corner trap
    3. At full skip the root would fall inside the near field, where amplitude cannot be relied on
    4. Half skip avoids the mode conversion that occurs whenever the beam reflects from the far surface
    Show the answer and explanation

    Answer: B. The root of a single-sided weld sits where the far surface meets the vertical face of an unfilled or unfused root. At half skip the beam arrives at that junction still on its first leg, and the two mutually perpendicular surfaces act as a corner reflector, sending energy straight back along the incoming path. That corner trap is what makes lack of penetration and root cracks such strong reflectors, and it is why root scanning is specified at half skip rather than left to chance. The attenuation option notices something true, that the path is shorter, but that is a secondary benefit rather than the reason. The near field option misplaces the near field, which is a property of the probe and its range, not of the leg being used, and the root at full skip would in any case be further away, not closer. The mode conversion option is wrong on the physics: reflection at the far surface does produce mode conversion, but that is not what half skip is avoiding.

  2. An aluminium honeycomb panel with bonded epoxy skins has to be checked for disbonds. Pulse echo from the skin returns a confusing train of echoes from inside the thin facesheet before anything reaches the bond line. What setup should be used?

    1. Through transmission with transmitter and receiver aligned on opposite faces, judging the bond by how much amplitude crosses the panel.
    2. A 10 MHz shear wave probe on the skin, because shear waves cross adhesive layers more efficiently than longitudinal waves do.
    3. A single 5 MHz angle beam probe on a long delay line, which pushes the facesheet echoes out beyond the gate that matters.
    4. An immersion setup with a focused probe gated on the third back wall echo returning from the far skin of the panel.
    Show the answer and explanation

    Answer: A. A thin facesheet rings, and in pulse echo the multiples from it crowd the very part of the timebase where the bond line signal would sit. Through transmission sidesteps the problem entirely: one probe sends, the other receives on the opposite face, and the measurement becomes how much energy gets across rather than what comes back. A disbond or a crushed core blocks that path and shows as a drop in transmitted amplitude, which is why bond testing of honeycomb and composite structure is normally done this way. Shear waves are not better at crossing an adhesive layer; they are heavily attenuated in adhesives and will not couple into air filled core at all. A longer delay line moves the interface echo but does not stop the facesheet ringing, so the multiples still land on top of the bond signal. Gating a third back wall echo assumes clean multiples through a panel that scarcely returns a first one.

Take the full free 10-question sample with scoring →

Frequently asked questions

Does ASNT publish how much of the UT exam is beam technique?

No. ASNT lists topics and tasks but does not release weights. A percentage you see for this area is an estimate, not an ASNT figure.

Which beam techniques does the new UT outline name?

For exams after February 5, 2027, the outline lists zero-degree, angle beam, pulse echo and through transmission as examples of the examinations a technician performs, for inherent, manufacturing and in-service discontinuities.

Is bonded structure still on the outline?

The outline for exams before February 5, 2027 lists evaluation of bonded structures as its own heading. The new outline does not use that heading, but the techniques it names still apply to bonded parts.

Official sources

  1. ASNT NDT Level II Examinations: Information and Scheduling — accessed 19 November 2026
  2. ASNT NDT Level II Certification: Foundational Credential — accessed 19 November 2026

Exam rules change. Check the awarding body's official page before you apply. CertCrafter is independent and is not affiliated with or endorsed by any awarding body.

Was this helpful?

Comments

    Comments are read by a person before they appear. How we moderate.